  • http://www.xcgdbearing.com/ lavede en statusopdatering 2 måneder, 3 uger siden

    The aluminum extrusion process starts with designing and creating the die that will shape the heatsink extrusion. Once this has been done, a cylindrical billet of aluminum is heated up in a forge to high temperatures, generally between 800-925°F (427-496°C). Next, a lubricant is added to the aluminum to prevent it from sticking to any of the machinery. It is then placed on a loader and pressure is applied with a ram to push heated aluminum through the die.